Bildunterschrift
Figure 3. The final atomic snapshots of the structured gold surface due to 400 fs laser pulse with 270 nm period intensity distribution along Y axis taken at t = 1000 ps The same incident fluence of 250 mJ/cm2 gives qualitatively different result for the case of structuring in air/vacuum (a) and under water layer (b) [10].